General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 2.4 - 2.5 g/cm³ Show Material materials with Densidad of 2.4 - 2.5 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Coeficiente de Poisson | 20.0 °C | 0.2 - 0.22 [-] Show Material materials with Coeficiente de Poisson of 0.2 - 0.22 [-] |
Dureza Knoop HK2 | 20.0 °C | 510 - 630 [-] Show Material materials with Dureza Knoop HK2 of 510 - 630 [-] |
Módulo elástico | 20.0 °C | 70 - 80 GPa Show Material materials with Módulo elástico of 70 - 80 GPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 20.0 °C | 0.68 - 0.87 J/(kg·K) Show Material materials with Calor específico of 0.68 - 0.87 J/(kg·K) | |
Coeficiente de dilatación térmica | 300.0 °C | 6.6E-6 - 9.3E-6 1/K Show Material materials with Coeficiente de dilatación térmica of 6.6E-6 - 9.3E-6 1/K | from 100 to 300°C |
Conductividad térmica | 20.0 °C | 0.18 - 1.32 W/(m·K) Show Material materials with Conductividad térmica of 0.18 - 1.32 W/(m·K) | |
Temperatura de transición del vidrio | 500 - 570 °C Show Material materials with Temperatura de transición del vidrio of 500 - 570 °C |
Óptico
Property | Value |
---|---|
Número de Abbe | 64.06 - 66.95 [-] Show Material materials with Número de Abbe of 64.06 - 66.95 [-] |
Índice de refracción | 1.5 - 1.52 [-] Show Material materials with Índice de refracción of 1.5 - 1.52 [-] |