General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 g/cm³ Show Material materials with Densidad of 7.8 g/cm³ | typical value |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | typical value |
Dureza Brinell | 23.0 °C | 321 - 363 [-] Show Material materials with Dureza Brinell of 321 - 363 [-] | in annealed condition: 197 |
Elongación | 23.0 °C | 10 % Show Material materials with Elongación of 10 % | |
Límite elástico | 23.0 °C | 930 MPa Show Material materials with Límite elástico of 930 MPa | |
Módulo elástico | 23.0 °C | 190 - 210 GPa Show Material materials with Módulo elástico of 190 - 210 GPa | typical value |
Resistencia a la tracción | 23.0 °C | 1080 - 1250 MPa Show Material materials with Resistencia a la tracción of 1080 - 1250 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 448 - 502 J/(kg·K) Show Material materials with Calor específico of 448 - 502 J/(kg·K) | Typical for Chromium Molybdenum Steel |
Coeficiente de dilatación térmica | 23.0 °C | 1.1E-5 - 1.4E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.1E-5 - 1.4E-5 1/K | Typical for Chromium Molybdenum Steel |
Conductividad térmica | 23.0 °C | 36 - 43 W/(m·K) Show Material materials with Conductividad térmica of 36 - 43 W/(m·K) | Typical for Chromium Molybdenum Steel |
Temperatura de fusión | 1382 - 1529 °C Show Material materials with Temperatura de fusión of 1382 - 1529 °C | Typical for Chromium Molybdenum Steel |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Azufre | 0.015 % Show Material materials with Azufre of 0.015 % | max. | |
Carbono | 0.12 - 0.18 % Show Material materials with Carbono of 0.12 - 0.18 % | ||
Cromo | 1.25 - 1.5 % Show Material materials with Cromo of 1.25 - 1.5 % | ||
Fósforo | 0.02 % Show Material materials with Fósforo of 0.02 % | max. | |
Hierro | Balance | ||
Manganeso | 0.8 - 1.1 % Show Material materials with Manganeso of 0.8 - 1.1 % | ||
Molibdeno | 0.8 - 1 % Show Material materials with Molibdeno of 0.8 - 1 % | ||
Silicona | 0.2 % Show Material materials with Silicona of 0.2 % | max. | |
Vanadio | 0.2 - 0.3 % Show Material materials with Vanadio of 0.2 - 0.3 % |
Technological properties
Property | ||
---|---|---|
Application areas | Pressure vessels, Wishbones, Uprights, Suspension components, Motorsport applications, Track and push rods, Rocket motor casings, Roll cages, Aerospace |