General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 g/cm³ Show Material materials with Densidad of 7.8 g/cm³ | typical value |
Medidas
Property | Value | Comment |
---|---|---|
Espesor | 200 mm Show Material materials with Espesor of 200 mm | max. |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | typical value |
Dureza Vickers | 23.0 °C | 270 - 300 [-] Show Material materials with Dureza Vickers of 270 - 300 [-] | |
Elongación | 23.0 °C | 40 % Show Material materials with Elongación of 40 % | min., A5.65 |
Energía de impacto Charpy | 23.0 °C | 180 J Show Material materials with Energía de impacto Charpy of 180 J | min. |
Límite elástico | 23.0 °C | 600 - 800 MPa Show Material materials with Límite elástico of 600 - 800 MPa | |
Módulo elástico | 23.0 °C | 190 - 210 GPa Show Material materials with Módulo elástico of 190 - 210 GPa | typical value |
Resistencia a la tracción | 23.0 °C | 900 - 1050 MPa Show Material materials with Resistencia a la tracción of 900 - 1050 MPa |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Azufre | 0.03 % Show Material materials with Azufre of 0.03 % | max. | |
Carbono | 0.12 % Show Material materials with Carbono of 0.12 % | max. | |
Cromo | 18 - 20 % Show Material materials with Cromo of 18 - 20 % | max. | |
Fósforo | 0.06 % Show Material materials with Fósforo of 0.06 % | max. | |
Hierro | Balance | ||
Manganeso | 9 - 11 % Show Material materials with Manganeso of 9 - 11 % | ||
Molibdeno | 1 % Show Material materials with Molibdeno of 1 % | max. | |
Nitrógeno | 0.4 - 0.65 % Show Material materials with Nitrógeno of 0.4 - 0.65 % | max | |
Níquel | 1 % Show Material materials with Níquel of 1 % | max. | |
Silicona | 1 % Show Material materials with Silicona of 1 % | max. |