General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 g/cm³ Show Material materials with Densidad of 7.8 g/cm³ | typical value |
Medidas
Property | Value |
---|---|
Espesor | 16 - 250 mm Show Material materials with Espesor of 16 - 250 mm |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | typical value |
Dureza Brinell | 23.0 °C | 248 [-] Show Material materials with Dureza Brinell of 248 [-] | max. |
Elongación | 23.0 °C | 11 - 13 % Show Material materials with Elongación of 11 - 13 % | min., A5.65 |
Energía de impacto Charpy | 23.0 °C | 30 - 45 J Show Material materials with Energía de impacto Charpy of 30 - 45 J | min. |
Límite elástico | 23.0 °C | 700 - 950 MPa Show Material materials with Límite elástico of 700 - 950 MPa | min. |
Módulo elástico | 23.0 °C | 190 - 210 GPa Show Material materials with Módulo elástico of 190 - 210 GPa | typical value |
Resistencia a la tracción | 23.0 °C | 900 - 1350 MPa Show Material materials with Resistencia a la tracción of 900 - 1350 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 470 J/(kg·K) Show Material materials with Calor específico of 470 J/(kg·K) | typical value |
Coeficiente de dilatación térmica | 23.0 °C | 1.3E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.3E-5 1/K | typical value |
Conductividad térmica | 23.0 °C | 39 W/(m·K) Show Material materials with Conductividad térmica of 39 W/(m·K) | typical value |
Eléctrico
Property | Value | Comment |
---|---|---|
Specific Electrical conductivity | 7.8 % IACS Show Material materials with Specific Electrical conductivity of 7.8 % IACS | typical value |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Azufre | 0.035 % Show Material materials with Azufre of 0.035 % | max. DIN EN ISO 683-17: 0.015 | |
Carbono | 0.29 - 0.36 % Show Material materials with Carbono of 0.29 - 0.36 % | ||
Cobre | 0.1 % Show Material materials with Cobre of 0.1 % | max. DIN EN ISO 683-17: 0.1-0.4 | |
Cromo | 2.8 - 3.3 % Show Material materials with Cromo of 2.8 - 3.3 % | ||
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % | max. | |
Hierro | Balance | ||
Manganeso | 0.4 - 0.7 % Show Material materials with Manganeso of 0.4 - 0.7 % | ||
Molibdeno | 0.7 - 1 % Show Material materials with Molibdeno of 0.7 - 1 % | DIN EN ISO 683-17: 0.7-1.2 | |
Níquel | 0.3 % Show Material materials with Níquel of 0.3 % | max. DIN EN ISO 683-17 | |
Silicona | 0.4 % Show Material materials with Silicona of 0.4 % | max. DIN EN ISO 683-17: 0.1-0.4 | |
Vanadio | 0.15 - 0.25 % Show Material materials with Vanadio of 0.15 - 0.25 % |