General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 g/cm³ Show Material materials with Densidad of 7.8 g/cm³ | typical value |
Medidas
Property | Value |
---|---|
Espesor | 16 - 100 mm Show Material materials with Espesor of 16 - 100 mm |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | typical value |
Dureza Brinell | 23.0 °C | 217 [-] Show Material materials with Dureza Brinell of 217 [-] | max. in soft annealed condition |
Elongación | 23.0 °C | 10 - 12 % Show Material materials with Elongación of 10 - 12 % | min., A5.65 |
Energía de impacto Charpy | 23.0 °C | 15 - 30 J Show Material materials with Energía de impacto Charpy of 15 - 30 J | |
Estricción | 23.0 °C | 30 - 40 % Show Material materials with Estricción of 30 - 40 % | min. |
Límite elástico | 23.0 °C | 685 - 885 MPa Show Material materials with Límite elástico of 685 - 885 MPa | |
Módulo elástico | 23.0 °C | 190 - 210 GPa Show Material materials with Módulo elástico of 190 - 210 GPa | typical value |
Resistencia a la tracción | 23.0 °C | 880 - 1270 MPa Show Material materials with Resistencia a la tracción of 880 - 1270 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 510 - 553 J/(kg·K) Show Material materials with Calor específico of 510 - 553 J/(kg·K) | Typical for Manganese Steel |
Coeficiente de dilatación térmica | 23.0 °C | 1.33E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.33E-5 1/K | Typical for Manganese Steel |
Conductividad térmica | 23.0 °C | 14 - 16 W/(m·K) Show Material materials with Conductividad térmica of 14 - 16 W/(m·K) | Typical for Manganese Steel |
Temperatura de fusión | 1382 - 1529 °C Show Material materials with Temperatura de fusión of 1382 - 1529 °C | Typical for Manganese Steel |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Azufre | 0.035 % Show Material materials with Azufre of 0.035 % | max. | |
Carbono | 0.38 - 0.45 % Show Material materials with Carbono of 0.38 - 0.45 % | ||
Fósforo | 0.04 % Show Material materials with Fósforo of 0.04 % | max. | |
Hierro | Balance | ||
Manganeso | 1.6 - 1.9 % Show Material materials with Manganeso of 1.6 - 1.9 % | ||
Silicona | 0.15 - 0.35 % Show Material materials with Silicona of 0.15 - 0.35 % | ||
Vanadio | 0.07 - 0.12 % Show Material materials with Vanadio of 0.07 - 0.12 % |