General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 8 g/cm³ Show Material materials with Densidad of 8 g/cm³ |
Medidas
Property | Value | Comment |
---|---|---|
Espesor | 50 mm Show Material materials with Espesor of 50 mm | max. |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | typical value |
Elongación | 23.0 °C | 30 % Show Material materials with Elongación of 30 % | min., A5.65 |
Energía de impacto Charpy | 23.0 °C | 60 J Show Material materials with Energía de impacto Charpy of 60 J | min. |
Límite elástico Rp 0,2 | 23.0 °C | 210 MPa Show Material materials with Límite elástico Rp 0,2 of 210 MPa | min. |
Límite elástico Rp0.1 | 23.0 °C | 235 MPa Show Material materials with Límite elástico Rp0.1 of 235 MPa | min. |
Módulo de cizallamiento | 23.0 °C | 77 GPa Show Material materials with Módulo de cizallamiento of 77 GPa | Typical for Austenitic Stainless Steel |
Módulo elástico | 23.0 °C | 190 - 210 GPa Show Material materials with Módulo elástico of 190 - 210 GPa | typical value |
Resistencia a la tracción | 23.0 °C | 480 MPa Show Material materials with Resistencia a la tracción of 480 MPa | min. |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 500 J/(kg·K) Show Material materials with Calor específico of 500 J/(kg·K) | |
Coeficiente de dilatación térmica | 100.0 °C | 1.65E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.65E-5 1/K | mean value between 20°C and the mentioned temperature |
200.0 °C | 1.75E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.75E-5 1/K | mean value between 20°C and the mentioned temperature | |
300.0 °C | 1.85E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.85E-5 1/K | mean value between 20°C and the mentioned temperature | |
Conductividad térmica | 50.0 °C | 15 W/(m·K) Show Material materials with Conductividad térmica of 15 W/(m·K) | |
100.0 °C | 16 W/(m·K) Show Material materials with Conductividad térmica of 16 W/(m·K) | ||
Temperatura de fusión | 1230 - 1480 °C Show Material materials with Temperatura de fusión of 1230 - 1480 °C | Typical for Austenitic Stainless Steel |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Resistividad eléctrica | 23.0 °C | 8.5E-7 Ω·m Show Material materials with Resistividad eléctrica of 8.5E-7 Ω·m | Typical for Austenitic Stainless Steel |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Azufre | 0.02 % Show Material materials with Azufre of 0.02 % | max. | |
Carbono | 0.025 % Show Material materials with Carbono of 0.025 % | max. | |
Cobre | 0.5 - 1.5 % Show Material materials with Cobre of 0.5 - 1.5 % | ||
Cromo | 19 - 21 % Show Material materials with Cromo of 19 - 21 % | ||
Fósforo | 0.04 % Show Material materials with Fósforo of 0.04 % | max. | |
Hierro | Balance | ||
Manganeso | 2 % Show Material materials with Manganeso of 2 % | max | |
Molibdeno | 6 - 7 % Show Material materials with Molibdeno of 6 - 7 % | ||
Nitrógeno | 0.1 - 0.25 % Show Material materials with Nitrógeno of 0.1 - 0.25 % | ||
Níquel | 24 - 26 % Show Material materials with Níquel of 24 - 26 % | ||
Silicona | 1 % Show Material materials with Silicona of 1 % | max. |