General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 7.75 g/cm³ Show Material materials with Densidad of 7.75 g/cm³ |
Mecánica
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 1.08E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.08E-5 1/K |
Conductividad térmica | 23.0 °C | 18.4 W/(m·K) Show Material materials with Conductividad térmica of 18.4 W/(m·K) |
Eléctrico
Property | Temperature | Value |
---|---|---|
Resistividad eléctrica | 23.0 °C | 8E-8 Ω·m Show Material materials with Resistividad eléctrica of 8E-8 Ω·m |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.9 - 1.35 % Show Material materials with Aluminio of 0.9 - 1.35 % |
Azufre | 0.01 % Show Material materials with Azufre of 0.01 % |
Carbono | 0.05 % Show Material materials with Carbono of 0.05 % |
Cromo | 12.25 - 13.25 % Show Material materials with Cromo of 12.25 - 13.25 % |
Fósforo | 0.01 % Show Material materials with Fósforo of 0.01 % |
Hierro | Balance |
Manganeso | 0.1 % Show Material materials with Manganeso of 0.1 % |
Molibdeno | 2 - 2.5 % Show Material materials with Molibdeno of 2 - 2.5 % |
Nitrógeno | 0.01 % Show Material materials with Nitrógeno of 0.01 % |
Níquel | 7.5 - 8.5 % Show Material materials with Níquel of 7.5 - 8.5 % |
Silicona | 0.1 % Show Material materials with Silicona of 0.1 % |
Technological properties
Property | ||
---|---|---|
Application areas | Landing Gear, Valves, Shafts, Petrochemical Components |