Matmatch uses cookies and similar technologies to improve your experience and measure your interactions with our website. We also use them to provide you more relevant information and improve our platform and search tools. If that’s okay, click “Accept all.” To change your preferences, click “Open cookie settings.” You will find more information about cookies on our privacy policy page.
Open cookie settings
Materiales
Categories
No estás conectado
Categories
Encontrar proveedores de metales
List Your Company
Case Studies
Tools
Sobre nosotros
M50 is a premium-melted alloy. It offers excellent resistance to multi-axial stresses and good resistance to oxidation. The product is refined using vacuuminduction melting (VIM) and vacuum-arc remelting (VAR) processes. It possesses high compressive strength suitable for a high speed steel tool. It also has a high degree of cleanliness therefore can be finished to a high luster. M50 is a bearing steel suitable for use within the missile and bearing industry, offering high wear resistance and strength at elevated temperatures. Bearings within aircrafts and gas turbines are other typical applications of this alloy. M50 could also be used in tooling applications where high levels of performance are required.
Los datos sobre este material han sido proporcionados por Matmatch.
See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.
All categories
Let us help you find the best supplier!
4130 Steel (Chromoly): Properties and Applications
440C Stainless Steel: Properties, Processing and Application
7Cr17MoV vs 7Cr17 Stainless Steel
A Guide to Rebar Sizes – an overview of steel reinforcement bars
AISI 304 (1.4301) Stainless Steel
AISI 316 Stainless Steel: Specification and Datasheet
ASTM A1018
ASTM A108 Carbon and Alloy Steel Bars
ASTM A479 Stainless Steel
ASTM A53 Carbon Steel Pipes
ASTM A564 Stainless Steel Age Hardened
Advanced High Strength Steel: Nomenclature, Grades, and Applications
Alloy Steel: Properties, Processing and Applications
Austenitic Stainless Steel: Properties, Applications and Grades
Carbon Steel: Properties, Production, Examples and Applications
Cold Rolled Steels
Difference between AISI 316, AISI 316L and AISI 316LN Stainless Steel
Duplex Stainless Steel: Properties, Standards, and Applications
Electrical Steel: Properties, Types, Production, and Applications
Ferritic Stainless Steel: Properties, Grades, and Applications
Hot Rolled Steels
Introduction to Steel Grades
JIS SCM435 equivalent materials
Machinability, Castability, Formability, Hardenability and Weldability of Steel
Maraging Steel: Properties, Processing, and Applications
Martensitic Stainless Steel: Properties, Grades, and Applications
Materials Used in Bearings
Materials Used in Bridges
Stainless Steel: Properties, Production, Examples and Applications
Top Stainless Steel Suppliers in Europe
What is ASTM A182 Grade F6a Stainless Steel?
What is ASTM A36?
What is ASTM A53?
What is EN 10025 Grade S235JR?
List your company on Matmatch now and reach engineers around the world looking for such materials.
Request more informationGeneral
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 7.87 g/cm³ Show Material materials with Densidad of 7.87 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Steel |
Módulo elástico | 23.0 °C | 190 - 210 GPa Show Material materials with Módulo elástico of 190 - 210 GPa | Typical for Steel |
Chemical properties
Property | Value |
---|---|
Carbono | 0 - 0.85 % Show Material materials with Carbono of 0 - 0.85 % |
Cromo | 0 - 4.1 % Show Material materials with Cromo of 0 - 4.1 % |
Hierro | Balance |
Manganeso | 0 - 0.3 % Show Material materials with Manganeso of 0 - 0.3 % |
Molibdeno | 0 - 4.25 % Show Material materials with Molibdeno of 0 - 4.25 % |
Silicona | 0 - 0.2 % Show Material materials with Silicona of 0 - 0.2 % |
Vanadio | 0 % Show Material materials with Vanadio of 0 % |
Wolframio | 1 % Show Material materials with Wolframio of 1 % |
MATMATCH
We connect engineers, product designers and procurement teams with the best materials and suppliers for their job.
EMPRESA
CONTÁCTANOS
Siebenbürger Str. 23, 86983 Lechbruck am See, Germany
© 2024 Plansee Composite Materials GmbH, All rights reserved.