General
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of friction | 0.1 [-] Show Material materials with Coefficient of friction of 0.1 [-] | ASTM D1894 | |
Densidad | 23.0 °C | 0.93 g/cm³ Show Material materials with Densidad of 0.93 g/cm³ | ASTM D1505 |
Mecánica
Óptico
Property | Value | Comment |
---|---|---|
Turbidez | 14 % Show Material materials with Turbidez of 14 % | ASTM D1003 |
Technological properties
Property | ||
---|---|---|
Application areas | General purpose film,Heavy duty film |