General
Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua | 23.0 °C | 0.6 % Show Material materials with Absorción de agua of 0.6 % | Sim. to ISO 62 | 80mil |
Densidad | 23.0 °C | 1.22 g/cm³ Show Material materials with Densidad of 1.22 g/cm³ | ISO 1183 |
Mecánica
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.48 [-] Show Material materials with Coeficiente de Poisson of 0.48 [-] | |||
Dureza Shore D | 23.0 °C | 63 [-] Show Material materials with Dureza Shore D of 63 [-] | max., ISO 7619-1 | ||
Elongación | 23.0 °C | 300 % Show Material materials with Elongación of 300 % | min. | ISO 527-1/-2 | ||
Elongation at yield | 23.0 °C | 27 % Show Material materials with Elongation at yield of 27 % | ISO 527-1/-2 | ||
Límite elástico | 23.0 °C | 19 MPa Show Material materials with Límite elástico of 19 MPa | ISO 527-1/-2 | ||
Módulo elástico | 23.0 °C | 0.26 GPa Show Material materials with Módulo elástico of 0.26 GPa | ISO 527-1/-2 | ||
Resistencia a desgarros | 23.0 °C | 158 kN/m Show Material materials with Resistencia a desgarros of 158 kN/m | ISO 34-1 | ||
Resistencia a desgarros transversal | 23.0 °C | 145 kN/m Show Material materials with Resistencia a desgarros transversal of 145 kN/m | ISO 34-1 | ||
Resistencia a la tracción | 23.0 °C | 41 MPa Show Material materials with Resistencia a la tracción of 41 MPa | ISO 527-1/-2 | ||
Resistencia al choque, ensayo Charpy entallado | -40.0 °C | 15 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy entallado of 15 kJ/m² | ISO 179/1eA | ||
-6.0 °C | 25 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy entallado of 25 kJ/m² | ISO 179/1eA | |||
23.0 °C | 110 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy entallado of 110 kJ/m² | ISO 179/1eA | |||
Resistencia al choque, ensayo Izod no entallado | -40.0 °C | 19 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod no entallado of 19 kJ/m² | ISO 180/1A | ||
23.0 °C | 81 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod no entallado of 81 kJ/m² | ISO 180/1A | |||
Resistencia al choque, ensayo Charpy no entallado | No Break @ 23°C, ISO 179/1eU |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Brittleness temperature | -100 °C Show Material materials with Brittleness temperature of -100 °C | ISO 974 | |||
Calor específico | 23.0 °C | 2160 J/(kg·K) Show Material materials with Calor específico of 2160 J/(kg·K) | of melt | ||
Difusividad térmica | 23.0 °C | 0 mm²/s Show Material materials with Difusividad térmica of 0 mm²/s | |||
Heat deflection temperature, 0.45 MPa | 85 °C Show Material materials with Heat deflection temperature, 0.45 MPa of 85 °C | ISO 75-1/-2 | |||
Heat deflection temperature, 1.80 MPa | 45 °C Show Material materials with Heat deflection temperature, 1.80 MPa of 45 °C | ISO 75-1/-2 | |||
Temperatura de fusión | 211 °C Show Material materials with Temperatura de fusión of 211 °C | ISO 11357-1/-3 | 18°F/min | |||
Temperatura de reblandecimiento Vicat | 195 °C Show Material materials with Temperatura de reblandecimiento Vicat of 195 °C | ISO 306 | 90°F, 2 lbf | |||
Inflamabilidad | FMVSS Class: B -, Burning rate, Thickness 1 mm: <80 mm/min |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Índice de seguimiento comparativo | 23.0 °C | 600 V Show Material materials with Índice de seguimiento comparativo of 600 V | IEC 60112 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 1.5 % Show Material materials with Contracción of 1.5 % | ISO 294-4, 2577 |
Contracción transversal | 23.0 °C | 1.5 % Show Material materials with Contracción transversal of 1.5 % | ISO 294-4, 2577 |
Velocidad de flujo de la masa derretida | 9 g/10min Show Material materials with Velocidad de flujo de la masa derretida of 9 g/10min | ISO 1133 | 230°C/2.16kg | |
Velocidad de flujo del volumen derretido | 8.5 cm³/10min Show Material materials with Velocidad de flujo del volumen derretido of 8.5 cm³/10min | ISO 1133 |
Technological properties
Property | ||
---|---|---|
Processing methods | Drying Recommended: yes, Drying Temperature: 100°C, Drying Time, Dehumidified Dryer: 2-3h, Processing Moisture Content: ≤0.08%, Melt Temperature Optimum: 240°C, Min. melt temperature: 235°C, Max. melt temperature: 260°C, Mold Temperature Optimum: 45°C, Min. mold temperature: 45°C, Max. mold temperature: 55°C, Hold pressure range: ≤70MPa |