Aplicaciones térmicas
Property | Value | Comment | |
---|---|---|---|
Temperatura de fusión | 154 °C Show Material materials with Temperatura de fusión of 154 °C | ISO 11357-1/-3 | 18°F/min | |
Inflamabilidad | FMVSS Class: B -, Burning rate, Thickness 1 mm: <80 mm/min |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Dissipation factor, 100Hz | 23.0 °C | 6E-3 [-] Show Material materials with Dissipation factor, 100Hz of 6E-3 [-] | IEC 62631-2-1 |
Dissipation factor, 1MHz | 23.0 °C | 0.01 [-] Show Material materials with Dissipation factor, 1MHz of 0.01 [-] | IEC 62631-2-1 |
Rigidez dieléctrica | 23.0 °C | 34 kV/mm Show Material materials with Rigidez dieléctrica of 34 kV/mm | IEC 60243-1 |
Volume resistivity | 23.0 °C | 1.00E+15 Ω·cm Show Material materials with Volume resistivity of 1.00E+15 Ω·cm | min. | IEC 62631-3-1 |
Índice de seguimiento comparativo | 23.0 °C | 300 V Show Material materials with Índice de seguimiento comparativo of 300 V | IEC 60112 |
Technological properties
Property | ||
---|---|---|
Fillers | Carbon Black | |
Processing methods | Drying Recommended: yes |