Hytrel® 4056P

Nombres alternativos y comerciales
TPC-ET
Want to keep this datasheet? Save it now in your required format

Description

Common features of Hytrel® thermoplastic polyester elastomer include mechanical and physical properties such as exceptional toughness and resilience, high resistance to creep, impact and flex fatigue, flexibility at low temperatures and good retention of properties at elevated temperatures. In addition, it resists many industrial chemicals, oils and solvents. Special grades include heat stabilised, flame retardant, food contact compliant, blow molding and extrusion grades. Concentrates offered include black pigments, UV protection additives, heat stabilisers, and flame retardants. Hytrel® thermoplastic polyester elastomer is plasticiser free.The good melt stability of Hytrel® thermoplastic polyester elastomer normally enables the recycling of properly handled production waste. If recycling is not possible, DuPont recommends, as the preferred option, incineration with energy recovery (-24 kJ/g of base polymer) in appropriately equipped installations.For disposal, local regulations have to be observed. Hytrel® thermoplastic polyester elastomer typically is used in demanding applications in the automotive, fluid power, electrical/electronic, consumer goods, appliance and power tool, sporting goods, furniture, industrial and off-road transportation/equipment industry.Hytrel® 4056P is a low modulus Hytrel® grade with nominal durometer hardness of 40D and with high impact resistance down to -40°C. It is delivered in a powder form.

Los datos sobre este material han sido proporcionados por Matmatch.

A menos que se indique lo contrario, todas las medidas corresponden a condiciones de temperatura ambiente. A menos que se indique lo contrario, se utilizan las unidades del SI.
Las normas armonizadas son similares a uno o varios estándares del proveedor. Es posible que algunas normas armonizadas se ajusten al estándar original, mientras que otras pueden quedar fuera de su alcance.

Ashby charts

Propiedades

Mecánica

PropertyTemperatureValueComment

Coeficiente de Poisson

23.0 °C

0.5 [-]

Show Material materials with Coeficiente de Poisson of 0.5 [-]

Dureza Shore D

23.0 °C

43 [-]

Show Material materials with Dureza Shore D of 43 [-]

max., ISO 7619-1

Elongación

23.0 °C

500 %

Show Material materials with Elongación of 500 %

ISO 527-1/-2

Módulo de flexión

23.0 °C

0.06 GPa

Show Material materials with Módulo de flexión of 0.06 GPa

ISO 178

Módulo elástico

23.0 °C

0.06 GPa

Show Material materials with Módulo elástico of 0.06 GPa

ISO 527-1/-2

Resistencia a desgarros

23.0 °C

102 kN/m

Show Material materials with Resistencia a desgarros of 102 kN/m

ISO 34-1

Resistencia a desgarros transversal

23.0 °C

96 kN/m

Show Material materials with Resistencia a desgarros transversal of 96 kN/m

ISO 34-1

Resistencia a la tracción

23.0 °C

26 MPa

Show Material materials with Resistencia a la tracción of 26 MPa

ISO 527-1/-2

Resistencia al choque, ensayo Charpy entallado

No Break @ 23,-6°C, ISO 179/1eA

Resistencia al choque, ensayo Charpy no entallado

No Break @ 23,-6°C,ISO 179/1eU

Aplicaciones térmicas

PropertyValueComment

Temperatura de fusión

152 °C

Show Material materials with Temperatura de fusión of 152 °C

ISO 11357-1/-3 | 18°F/min

Temperatura de transición del vidrio

-50 °C

Show Material materials with Temperatura de transición del vidrio of -50 °C

ISO 11357-1/-2 | 18°F/min

Inflamabilidad

FMVSS Class: B -, Burning rate, Thickness 1 mm: <80 mm/min

Eléctrico

PropertyTemperatureValueComment

Índice de seguimiento comparativo

23.0 °C

600 V

Show Material materials with Índice de seguimiento comparativo of 600 V

IEC 60112

Rheological Properties

PropertyValueComment

Velocidad de flujo de la masa derretida

5.6 g/10min

Show Material materials with Velocidad de flujo de la masa derretida of 5.6 g/10min

ISO 1133 | 190°C/2.16kg

Velocidad de flujo del volumen derretido

5 cm³/10min

Show Material materials with Velocidad de flujo del volumen derretido of 5 cm³/10min

ISO 1133

Technological properties

Property
Processing methods

Drying Recommended: yes, Drying Temperature: 80°C, Drying Time, Dehumidified Dryer: 2-3h, Processing Moisture Content: ≤0.08%