Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.48 [-] Show Material materials with Coeficiente de Poisson of 0.48 [-] | |
Dureza Shore D | 23.0 °C | 55 [-] Show Material materials with Dureza Shore D of 55 [-] | max., ISO 7619-1 |
Elongación | 23.0 °C | 300 % Show Material materials with Elongación of 300 % | min. | ISO 527-1/-2 |
Módulo de flexión | 23.0 °C | 0.21 GPa Show Material materials with Módulo de flexión of 0.21 GPa | ISO 178 |
Módulo elástico | 23.0 °C | 0.23 GPa Show Material materials with Módulo elástico of 0.23 GPa | ISO 527-1/-2 |
Resistencia a desgarros | 23.0 °C | 160 kN/m Show Material materials with Resistencia a desgarros of 160 kN/m | ISO 34-1 |
Resistencia a desgarros transversal | 23.0 °C | 140 kN/m Show Material materials with Resistencia a desgarros transversal of 140 kN/m | ISO 34-1 |
Resistencia a la tracción | 23.0 °C | 33.6 MPa Show Material materials with Resistencia a la tracción of 33.6 MPa | ISO 527-1/-2 |
Resistencia al choque, ensayo Charpy entallado | -40.0 °C | 26.6 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy entallado of 26.6 kJ/m² | No Break @ 23°C, ISO 179/1eA |
-6.0 °C | 150 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy entallado of 150 kJ/m² | No Break @ 23°C, ISO 179/1eA | |
Aplicaciones térmicas
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 1.2 % Show Material materials with Contracción of 1.2 % | ISO 294-4, 2577 |
Contracción transversal | 23.0 °C | 1.6 % Show Material materials with Contracción transversal of 1.6 % | ISO 294-4, 2577 |
Velocidad de flujo de la masa derretida | 5.9 g/10min Show Material materials with Velocidad de flujo de la masa derretida of 5.9 g/10min | ISO 1133 | 230°C/10kg |
Technological properties
Property | ||
---|---|---|
Processing methods | Drying Recommended: yes, Drying Temperature: 100°C, Drying Time, Dehumidified Dryer: 2-4h, Processing Moisture Content: ≤0.08%, Melt Temperature Optimum: 240°C, Min. melt temperature: 230°C, Max. melt temperature: 250°C, Mold Temperature Optimum: 45°C, Min. mold temperature: 40°C, Max. mold temperature: 50°C |