General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.18 g/cm³ Show Material materials with Densidad of 1.18 g/cm³ | ISO 1183 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Shore A | 23.0 °C | 45 [-] Show Material materials with Dureza Shore A of 45 [-] | ISO 7619-1 | 3 seconds |
Elongación | 23.0 °C | 750 % Show Material materials with Elongación of 750 % | ISO 527-1/-2 |
Resistencia a desgarros | 23.0 °C | 20 kN/m Show Material materials with Resistencia a desgarros of 20 kN/m | ISO 34-1 |
Resistencia a la tracción | 23.0 °C | 5 MPa Show Material materials with Resistencia a la tracción of 5 MPa | ISO 527-1/-2 |
Set de compresión | 23.0 °C | 13 [-] Show Material materials with Set de compresión of 13 [-] | ISO 815 |
70.0 °C | 38 [-] Show Material materials with Set de compresión of 38 [-] | ISO 815 | |
100.0 °C | 66 [-] Show Material materials with Set de compresión of 66 [-] | ISO 815 | |
Technological properties
Property | ||
---|---|---|
Color | Black | |
Processing methods | Drying Recommended: no, Melt Temperature Optimum: 210°C, Mold Temperature Optimum: 40°C, Min. mold temperature: 20°C, Max. mold temperature: 60°C, Hold pressure range: as low as possible, Back pressure: 1MPa |