General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 0.91 g/cm³ Show Material materials with Densidad of 0.91 g/cm³ | ISO 1183 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Shore D | 23.0 °C | 34 [-] Show Material materials with Dureza Shore D of 34 [-] | ISO 7619-1 | 15 seconds |
Elongación | 23.0 °C | 180 % Show Material materials with Elongación of 180 % | ISO 527-1/-2 |
Módulo de flexión | 23.0 °C | 0.28 GPa Show Material materials with Módulo de flexión of 0.28 GPa | ISO 178 |
Resistencia a desgarros | 23.0 °C | 75 kN/m Show Material materials with Resistencia a desgarros of 75 kN/m | ISO 34-1 |
Resistencia a la tracción | 23.0 °C | 13.5 MPa Show Material materials with Resistencia a la tracción of 13.5 MPa | ISO 527-1/-2 |
Resistencia al choque, ensayo Izod no entallado | -50.0 °C | 67 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod no entallado of 67 kJ/m² | ISO 180/1A |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 1.2 % Show Material materials with Contracción of 1.2 % | ISO 294-4, 2577 |
Velocidad de flujo del volumen derretido | 4.5 cm³/10min Show Material materials with Velocidad de flujo del volumen derretido of 4.5 cm³/10min | ISO 1133 |
Technological properties
Property | ||
---|---|---|
Color | Black | |
Processing methods | Drying Recommended: no, Melt Temperature Optimum: 245°C, Mold Temperature Optimum: 30°C, Min. mold temperature: 20°C, Max. mold temperature: 40°C, Hold pressure range: as low as possible, Back pressure: 1MPa |