General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.04 g/cm³ Show Material materials with Densidad of 1.04 g/cm³ | ISO 1183 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Shore A | 23.0 °C | 25 [-] Show Material materials with Dureza Shore A of 25 [-] | ISO 7619-1 | 3 seconds |
Elongación | 23.0 °C | 650 % Show Material materials with Elongación of 650 % | ISO 527-1/-2 |
Resistencia a desgarros | 23.0 °C | 14 kN/m Show Material materials with Resistencia a desgarros of 14 kN/m | ISO 34-1 |
Resistencia a la tracción | 23.0 °C | 3.5 MPa Show Material materials with Resistencia a la tracción of 3.5 MPa | ISO 527-1/-2 |
Set de compresión | 23.0 °C | 8 [-] Show Material materials with Set de compresión of 8 [-] | ISO 815 |
70.0 °C | 22 [-] Show Material materials with Set de compresión of 22 [-] | ISO 815 | |
100.0 °C | 34 [-] Show Material materials with Set de compresión of 34 [-] | ISO 815 | |
Technological properties
Property | ||
---|---|---|
Processing methods | Drying Recommended: no, Melt Temperature Optimum: 210°C, Mold Temperature Optimum: 40°C, Min. mold temperature: 20°C, Max. mold temperature: 60°C, Hold pressure range: as low as possible, Back pressure: 1MPa |