General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.1 g/cm³ Show Material materials with Densidad of 1.1 g/cm³ | ISO 1183 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Shore A | 23.0 °C | 62 [-] Show Material materials with Dureza Shore A of 62 [-] | ISO 7619-1 | 3 seconds |
Elongación | 23.0 °C | 600 % Show Material materials with Elongación of 600 % | ISO 527-1/-2 |
Módulo de flexión | 23.0 °C | 0.02 GPa Show Material materials with Módulo de flexión of 0.02 GPa | ISO 178 |
Resistencia a desgarros transversal | 23.0 °C | 30 kN/m Show Material materials with Resistencia a desgarros transversal of 30 kN/m | ISO 34-1 |
Resistencia a la flexión | 23.0 °C | 1.51 MPa Show Material materials with Resistencia a la flexión of 1.51 MPa | ISO 178 |
Resistencia a la tracción | 23.0 °C | 5.2 MPa Show Material materials with Resistencia a la tracción of 5.2 MPa | ISO 527-1/-2 |
Set de compresión | 23.0 °C | 33 [-] Show Material materials with Set de compresión of 33 [-] | ISO 815 |
70.0 °C | 87 [-] Show Material materials with Set de compresión of 87 [-] | ISO 815 | |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 2.5 % Show Material materials with Contracción of 2.5 % | ISO 294-4, 2577 |
Velocidad de flujo de la masa derretida | 20 g/10min Show Material materials with Velocidad de flujo de la masa derretida of 20 g/10min | ISO 1133 | 190°C/10kg |
Technological properties
Property | ||
---|---|---|
Processing methods | Drying Recommended: yes, Drying Temperature: 85°C, Drying Time, Dehumidified Dryer: 2-4h, Melt Temperature Optimum: 190°C, Max. screw tangential speed: 0.4m/s, Mold Temperature Optimum: 30°C, Min. mold temperature: 20°C, Max. mold temperature: 40°C |