General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 0.92 g/cm³ Show Material materials with Densidad of 0.92 g/cm³ | ISO 1183 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Shore A | 23.0 °C | 60 [-] Show Material materials with Dureza Shore A of 60 [-] | ISO 7619-1 | 3 seconds |
Elongación | 23.0 °C | 845 % Show Material materials with Elongación of 845 % | ISO 527-1/-2 |
Resistencia a desgarros transversal | 23.0 °C | 44 kN/m Show Material materials with Resistencia a desgarros transversal of 44 kN/m | ISO 34-1 |
Resistencia a la tracción | 23.0 °C | 7.4 MPa Show Material materials with Resistencia a la tracción of 7.4 MPa | ISO 527-1/-2 |
Technological properties
Property | ||
---|---|---|
Processing methods | Drying Recommended: no, Mold Temperature Optimum: 30°C, Min. mold temperature: 28°C, Max. mold temperature: 32°C |