General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.18 g/cm³ Show Material materials with Densidad of 1.18 g/cm³ | ISO 1183 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Shore A | 23.0 °C | 73 [-] Show Material materials with Dureza Shore A of 73 [-] | ISO 7619-1 | 3 seconds |
Elongación | 23.0 °C | 554 % Show Material materials with Elongación of 554 % | ISO 527-1/-2 |
Módulo de flexión | 23.0 °C | 0.03 GPa Show Material materials with Módulo de flexión of 0.03 GPa | ISO 178 |
Resistencia a desgarros transversal | 23.0 °C | 48.6 kN/m Show Material materials with Resistencia a desgarros transversal of 48.6 kN/m | ISO 34-1 |
Resistencia a la flexión | 23.0 °C | 2.4 MPa Show Material materials with Resistencia a la flexión of 2.4 MPa | ISO 178 |
Resistencia a la tracción | 23.0 °C | 14.5 MPa Show Material materials with Resistencia a la tracción of 14.5 MPa | ISO 527-1/-2 |
Set de compresión | 23.0 °C | 22 [-] Show Material materials with Set de compresión of 22 [-] | ISO 815 |
70.0 °C | 75 [-] Show Material materials with Set de compresión of 75 [-] | ISO 815 | |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 2 % Show Material materials with Contracción of 2 % | ISO 294-4, 2577 |
Velocidad de flujo de la masa derretida | 27 g/10min Show Material materials with Velocidad de flujo de la masa derretida of 27 g/10min | ISO 1133 | 230°C/10kg |
Technological properties
Property | ||
---|---|---|
Processing methods | Drying Recommended: yes, Drying Temperature: 70°C, Drying Time, Dehumidified Dryer: 2-4h, Melt Temperature Optimum: 195°C, Max. screw tangential speed: 0.4m/s, Mold Temperature Optimum: 30°C, Min. mold temperature: 20°C, Max. mold temperature: 40°C |