Hytrel® PC938 NC010

Nombres alternativos y comerciales
TPC-ET
Want to keep this datasheet? Save it now in your required format

Description

Common features of Hytrel® thermoplastic polyester elastomer include mechanical and physical properties such as exceptional toughness and resilience, high resistance to creep, impact and flex fatigue, flexibility at low temperatures and good retention of properties at elevated temperatures. In addition, it resists many industrial chemicals, oils and solvents. Special grades include heat stabilised, flame retardant, food contact compliant, blow molding and extrusion grades. Concentrates offered include black pigments, UV protection additives, heat stabilisers, and flame retardants. Hytrel® thermoplastic polyester elastomer is plasticiser free.The good melt stability of Hytrel® thermoplastic polyester elastomer normally enables the recycling of properly handled production waste. If recycling is not possible, DuPont recommends, as the preferred option, incineration with energy recovery (-24 kJ/g of base polymer) in appropriately equipped installations.For disposal, local regulations have to be observed. Hytrel® thermoplastic polyester elastomer typically is used in demanding applications in the automotive, fluid power, electrical/electronic, consumer goods, appliance and power tool, sporting goods, furniture, industrial and off-road transportation/equipment industry.Hytrel® PC938 has a very low modulus, nominal hardness of 30D, containing non-discoloring stabilizer. Processed by thermoplastic processing techniques like injection molding and extrusion. Developed for applications such as parts for the healthcare industry.PREMIUM CONTROL for HEALTHCARE APPLICATIONSThis product is manufactured according to Good Manufacturing Practice (GMP) principles and generally accepted in food contact applications in the USA when meeting applicable use conditions. This product is also tested against ISO 10993-5 and -11 and selected parts of USP Class VI and FDA drug and device master files (DMF and MAF) have been established.For details, individual compliance statements are available from your DuPont representative.The below datasheet is a condensed version. For a complete datasheet, please contact your DuPont representative.

Los datos sobre este material han sido proporcionados por Matmatch.

A menos que se indique lo contrario, todas las medidas corresponden a condiciones de temperatura ambiente. A menos que se indique lo contrario, se utilizan las unidades del SI.
Las normas armonizadas son similares a uno o varios estándares del proveedor. Es posible que algunas normas armonizadas se ajusten al estándar original, mientras que otras pueden quedar fuera de su alcance.

Ashby charts

Propiedades

General

PropertyTemperatureValueComment

Densidad

23.0 °C

1.07 g/cm³

Show Material materials with Densidad of 1.07 g/cm³

ISO 1183

Mecánica

PropertyTemperatureValueComment

Dureza Shore D

23.0 °C

30 [-]

Show Material materials with Dureza Shore D of 30 [-]

max., ISO 7619-1

Elongación

23.0 °C

300 %

Show Material materials with Elongación of 300 %

min. | ISO 527-1/-2

Resistencia a la tracción

23.0 °C

24 MPa

Show Material materials with Resistencia a la tracción of 24 MPa

ISO 527-1/-2

Resistencia al choque, ensayo Charpy entallado

No Break @ 23°C, ISO 179/1eU

Aplicaciones térmicas

PropertyValueComment

Temperatura de fusión

177 °C

Show Material materials with Temperatura de fusión of 177 °C

ISO 11357-1/-3 | 18°F/min

Inflamabilidad

FMVSS Class: B -, Burning rate, Thickness 1 mm: <80 mm/min