General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.18 g/cm³ Show Material materials with Densidad of 1.18 g/cm³ | ISO 1183 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Shore A | 23.0 °C | 60 [-] Show Material materials with Dureza Shore A of 60 [-] | ISO 7619-1 | 3 seconds |
Elongación | 23.0 °C | 650 % Show Material materials with Elongación of 650 % | ISO 527-1/-2 |
Resistencia a desgarros | 23.0 °C | 23 kN/m Show Material materials with Resistencia a desgarros of 23 kN/m | ISO 34-1 |
Resistencia a la tracción | 23.0 °C | 5 MPa Show Material materials with Resistencia a la tracción of 5 MPa | ISO 527-1/-2 |
Rheological Properties
Technological properties
Property |
---|