General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.23 g/cm³ Show Material materials with Densidad of 1.23 g/cm³ | ISO 1183 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.48 [-] Show Material materials with Coeficiente de Poisson of 0.48 [-] | |
Dureza Shore D | 23.0 °C | 64 [-] Show Material materials with Dureza Shore D of 64 [-] | max., ISO 7619-1 |
Elongación | 23.0 °C | 480 % Show Material materials with Elongación of 480 % | ISO 527-1/-2 |
Elongation at yield | 23.0 °C | 30 % Show Material materials with Elongation at yield of 30 % | ISO 527-1/-2 |
Límite elástico | 23.0 °C | 21 MPa Show Material materials with Límite elástico of 21 MPa | ISO 527-1/-2 |
Módulo de flexión | 23.0 °C | 0.35 GPa Show Material materials with Módulo de flexión of 0.35 GPa | ISO 178 |
Módulo elástico | 23.0 °C | 0.34 GPa Show Material materials with Módulo elástico of 0.34 GPa | ISO 527-1/-2 |
Resistencia a desgarros | 23.0 °C | 200 kN/m Show Material materials with Resistencia a desgarros of 200 kN/m | ISO 34-1 |
Resistencia a desgarros transversal | 23.0 °C | 185 kN/m Show Material materials with Resistencia a desgarros transversal of 185 kN/m | ISO 34-1 |
Resistencia a la tracción | 23.0 °C | 44 MPa Show Material materials with Resistencia a la tracción of 44 MPa | ISO 527-1/-2 |
Resistencia al choque, ensayo Charpy entallado | -40.0 °C | 8.5 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy entallado of 8.5 kJ/m² | ISO 179/1eA |
-6.0 °C | 12 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy entallado of 12 kJ/m² | ISO 179/1eA | |
23.0 °C | 130 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy entallado of 130 kJ/m² | ISO 179/1eA | |
Resistencia al choque, ensayo Izod no entallado | -40.0 °C | 7.5 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod no entallado of 7.5 kJ/m² | No Break @ 23°C, ISO 179/1eU |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Brittleness temperature | -70 °C Show Material materials with Brittleness temperature of -70 °C | ISO 974 | |||
Calor específico | 23.0 °C | 2090 J/(kg·K) Show Material materials with Calor específico of 2090 J/(kg·K) | of melt | ||
Coeficiente de dilatación térmica | 23.0 °C | 2.2E-4 1/K Show Material materials with Coeficiente de dilatación térmica of 2.2E-4 1/K | ISO 11359-1/-2 | ||
Coeficiente de dilatación térmica transversal | 23.0 °C | 1.7E-4 1/K Show Material materials with Coeficiente de dilatación térmica transversal of 1.7E-4 1/K | ISO 11359-1/-2 | ||
Heat deflection temperature, 0.45 MPa | 85 °C Show Material materials with Heat deflection temperature, 0.45 MPa of 85 °C | ISO 75-1/-2 | |||
Temperatura de fusión | 210 °C Show Material materials with Temperatura de fusión of 210 °C | ISO 11357-1/-3 | 18°F/min | |||
Temperatura de reblandecimiento Vicat | 196 °C Show Material materials with Temperatura de reblandecimiento Vicat of 196 °C | ISO 306 | 90°F, 2 lbf | |||
Inflamabilidad | FMVSS Class: SE -, Burning rate, Thickness 1 mm: 17 mm/min |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 1.9 % Show Material materials with Contracción of 1.9 % | ISO 294-4, 2577 |
Contracción transversal | 23.0 °C | 1.8 % Show Material materials with Contracción transversal of 1.8 % | ISO 294-4, 2577 |
Velocidad de flujo del volumen derretido | 5 cm³/10min Show Material materials with Velocidad de flujo del volumen derretido of 5 cm³/10min | ISO 1133 |
Technological properties
Property | ||
---|---|---|
Processing methods | Drying Recommended: yes, Drying Temperature: 110°C, Drying Time, Dehumidified Dryer: 2-4h, Processing Moisture Content: ≤0.08%, Melt Temperature Optimum: 240°C, Min. melt temperature: 230°C, Max. melt temperature: 260°C, Mold Temperature Optimum: 45°C, Min. mold temperature: 45°C, Max. mold temperature: 55°C |