BS CZ101 (CW501L) Gilding Metal

View suppliers (10)
Want to keep this datasheet? Save it now in your required format

Description

2.0230 (CuZn10) is a brass alloy containing approximately 90% copper and 10% zinc. It is primarily supplied as a sheet grade and is classed as a gilding metal. The alloy offers excellent cold working properties and is generally not susceptible to dezincification or stress corrosion. Due to its formability and its attractive rich golden colour, CZ101 (CW501L) is widely used for architectural and decorative applications. It is also readily brazed and enamelled. It shows the following features and properties:


  • Excellent cold formability
  • High resistance to stress corrosion and dezincification
  • Related Standards

    Equivalent Materials

    Los datos sobre este material han sido proporcionados por Matmatch.

    A menos que se indique lo contrario, todas las medidas corresponden a condiciones de temperatura ambiente. A menos que se indique lo contrario, se utilizan las unidades del SI.
    Las normas armonizadas son similares a uno o varios estándares del proveedor. Es posible que algunas normas armonizadas se ajusten al estándar original, mientras que otras pueden quedar fuera de su alcance.

    Ashby charts

    Propiedades

    Chemical properties

    PropertyValue

    Cobre

    90 %

    Show Material materials with Cobre of 90 %

    Zinc

    10 %

    Show Material materials with Zinc of 10 %

    Technological properties

    Property
    Application areas

    Offshore & marine: Hardware, rivets and screws, wire gauzes and slide and zip fasteners;Architectural: Showcase and window fittings, decorative metalwork, roofing panels, grillwork, weatherstrip, cold-formed angles and channels, ornamental pressing and trim;Decorative: Cosmetic compacts and cases, costume jewellery, emblems, medallions and other items requiring vitreous enamelling

    Cold Forming

    Excellent cold working properties

    Corrosion properties

    High corrosion resistance