Chemical properties
Technological properties
Property | ||
---|---|---|
Application areas | Electrical: Lamp caps, lamp-holder and switch components;General: Coppersmithing work for chains, eyelets fasteners, hinges, kicking plates, locks, fingerplates and wire brushes, various cold presswork products including instrument covers and containers, blanked articles such as instrument plates and wheels, cold headed items including pins, rivets and screws, springs, radiator tanks and reflectors | |
Cold Forming | Good cold formability | |
Corrosion properties | Very good corrosion resistance | |
General machinability | Good machinability | |
Hot forming | Very good hot working capabilities. |