Mecánica
Property | Temperature | Value |
---|---|---|
Elongación | 23.0 °C | 15 - 20 % Show Material materials with Elongación of 15 - 20 % |
Resistencia a la tracción | 23.0 °C | 350 - 400 MPa Show Material materials with Resistencia a la tracción of 350 - 400 MPa |
Chemical properties
Technological properties
Property | ||
---|---|---|
Application areas | Offshore & marine: Marine hardware, tube plates and fasteners for corrosion-resistant service;Other: High strength cold-headed products and fasteners | |
Corrosion properties | High corrosion resistance for marine hardware and other mildly aggressive environments. | |
Hot forming | Excellent hot formability. |