Matmatch uses cookies and similar technologies to improve your experience and measure your interactions with our website. We also use them to provide you more relevant information and improve our platform and search tools. If that’s okay, click “Accept all.” To change your preferences, click “Open cookie settings.” You will find more information about cookies on our privacy policy page.
Open cookie settings
Materiales
Categories
No estás conectado
Categories
Encontrar proveedores de metales
List Your Company
Case Studies
Tools
Sobre nosotros
BS CZ120 (CW608N) Engraving Brass
2.0380 (CuZn38Pb2) also known as engraving brass, is a classic leaded machining alloy primarily available in sheet form. It is an alpha beta brass with a 2% lead addition that gives the alloy its free-cutting properties. Traditionally used for machine-engraved nameplates and signs. It also offers a good combination of strength, corrosion resistance and hot formability. The duplex phase structure, however, means this alloy is not suitable for acid-etched work. It shows the following features and properties:
Los datos sobre este material han sido proporcionados por Matmatch.
All categories
Suppliers with similar grades
Properties of Copper
List your company on Matmatch now and reach engineers around the world looking for such materials.
Request more informationChemical properties
Technological properties
Property | ||
---|---|---|
Application areas | Decorative & architectural: Signs, nameplates, door furniture, window fittings, valve and pump parts, decorative metalwork, clock and instrument casings, gears, cams and fasteners | |
Corrosion properties | High corrosion resistance | |
General machinability | Very good | |
Hot forming | Excellent hot formability |
MATMATCH
We connect engineers, product designers and procurement teams with the best materials and suppliers for their job.
EMPRESA
CONTÁCTANOS
Siebenbürger Str. 23, 86983 Lechbruck am See, Germany
© 2024 Plansee Composite Materials GmbH, All rights reserved.