Mecánica
Property | Temperature | Value |
---|---|---|
Elongación | 23.0 °C | 15 - 25 % Show Material materials with Elongación of 15 - 25 % |
Resistencia a la tracción | 23.0 °C | 350 - 425 MPa Show Material materials with Resistencia a la tracción of 350 - 425 MPa |
Chemical properties
Technological properties
Property | ||
---|---|---|
Application areas | General: A wide variety of machined components usually made on high speed automatic lathes including nuts, bolts, screws, bushings, bearings, pins and washers, plug pins, switch terminals, lock bodies, hinges, extruded sections, door treads, window frames and trim | |
Corrosion properties | Good corrosion resistance | |
General machinability | Machinability rating: 100% |