Mecánica
Property | Temperature | Value |
---|---|---|
Elongación | 23.0 °C | 25 - 40 % Show Material materials with Elongación of 25 - 40 % |
Límite elástico | 23.0 °C | 440 - 510 MPa Show Material materials with Límite elástico of 440 - 510 MPa |
Resistencia a la tracción | 23.0 °C | 540 - 590 MPa Show Material materials with Resistencia a la tracción of 540 - 590 MPa |
Chemical properties
Technological properties
Property | ||
---|---|---|
Application areas | Offshore & marine: Decorative trim, marine hardware and sheathing.;Aerospace: Cold workable components.;Other: Architectural panels and decorative trim, coinage, storage tanks, heat exchangers, water boxes, munitions mixing chambers, masonry fixings and non-magnetic instrument casings | |
Cold Forming | Excellent cold working properties | |
Corrosion properties | Excellent corrosion resistance |