General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 7.5 g/cm³ Show Material materials with Densidad of 7.5 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Charpy impact energy, V-notch | 23.0 °C | 27 J Show Material materials with Charpy impact energy, V-notch of 27 J |
Elongación | 23.0 °C | 17 % Show Material materials with Elongación of 17 % |
Límite elástico Rp 0,2 | 23.0 °C | 245 - 325 MPa Show Material materials with Límite elástico Rp 0,2 of 245 - 325 MPa |
Resistencia a la tracción | 23.0 °C | 620 - 680 MPa Show Material materials with Resistencia a la tracción of 620 - 680 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 1.8E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.8E-5 1/K | for 0-300°C |
Conductividad térmica | 23.0 °C | 59 - 67 W/(m·K) Show Material materials with Conductividad térmica of 59 - 67 W/(m·K) | |
Temperatura de fusión | 1060 - 1075 °C Show Material materials with Temperatura de fusión of 1060 - 1075 °C |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 23.0 °C | 6.96E+6 - 8.12E+6 S/m Show Material materials with Conductividad eléctrica of 6.96E+6 - 8.12E+6 S/m |
Specific Electrical conductivity | 12 - 14 % IACS Show Material materials with Specific Electrical conductivity of 12 - 14 % IACS |
Magnético
Property | Temperature | Value |
---|---|---|
Permeabilidad magnética relativa | 23.0 °C | 1.5 [-] Show Material materials with Permeabilidad magnética relativa of 1.5 [-] |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminio | 8.5 - 10 % Show Material materials with Aluminio of 8.5 - 10 % | ||
Cobre | Balance | ||
Hierro | 4 - 5 % Show Material materials with Hierro of 4 - 5 % | ||
Manganeso | 0.5 % Show Material materials with Manganeso of 0.5 % | max. | |
Níquel | 4.5 - 5.5 % Show Material materials with Níquel of 4.5 - 5.5 % |
Technological properties
Property | ||
---|---|---|
Application areas | Offshore & marine: High performance fasteners, valve and pump components, propeller shafts and weapons handling systems;Other: Pipe fittings, heat exchangers, wear plates, thrust washers, bearings, bushes, safety tools, worm wheels and gears | |
Corrosion properties | Excellent resistance to erosion and corrosion |