Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 23.0 °C | 200 - 220 [-] Show Material materials with Dureza Brinell of 200 - 220 [-] |
Elongación | 23.0 °C | 10 - 13 % Show Material materials with Elongación of 10 - 13 % |
Límite elástico | 23.0 °C | 400 - 500 MPa Show Material materials with Límite elástico of 400 - 500 MPa |
Resistencia a la tracción | 23.0 °C | 700 - 760 MPa Show Material materials with Resistencia a la tracción of 700 - 760 MPa |
Chemical properties
Property | Value |
---|---|
Aluminio | 9.7 % Show Material materials with Aluminio of 9.7 % |
Cobre | Balance |
Hierro | 3.8 % Show Material materials with Hierro of 3.8 % |
Manganeso | 1.3 % Show Material materials with Manganeso of 1.3 % |
Níquel | 5 % Show Material materials with Níquel of 5 % |
Plomo | 1.75 % Show Material materials with Plomo of 1.75 % |
Technological properties
Property | ||
---|---|---|
Application areas | Offshore & marine: Marine hardware, fasteners and fittings;General: Fasteners, gears, non-sparking safety tooling, thrust washers, valve guides, fluid handling equipment, valve spindles and components, bearings pins and bushes, thermostatic valves and worm wheels | |
Corrosion properties | Excellent general corrosion resistance | |
General machinability | Excellent machinability |