General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 7.6 g/cm³ Show Material materials with Densidad of 7.6 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Elongación | 23.0 °C | 5 - 12 % Show Material materials with Elongación of 5 - 12 % |
Límite elástico Rp 0,2 | 23.0 °C | 275 - 415 MPa Show Material materials with Límite elástico Rp 0,2 of 275 - 415 MPa |
Resistencia a la tracción | 23.0 °C | 550 - 760 MPa Show Material materials with Resistencia a la tracción of 550 - 760 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 1.7E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.7E-5 1/K | for 0-300°C |
Conductividad térmica | 23.0 °C | 38 - 46 W/(m·K) Show Material materials with Conductividad térmica of 38 - 46 W/(m·K) | |
Temperatura de fusión | 1050 - 1070 °C Show Material materials with Temperatura de fusión of 1050 - 1070 °C |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 23.0 °C | 4.06E+6 - 5.22E+6 S/m Show Material materials with Conductividad eléctrica of 4.06E+6 - 5.22E+6 S/m |
Specific Electrical conductivity | 7 - 9 % IACS Show Material materials with Specific Electrical conductivity of 7 - 9 % IACS |
Magnético
Property | Temperature | Value |
---|---|---|
Permeabilidad magnética relativa | 23.0 °C | 1 [-] Show Material materials with Permeabilidad magnética relativa of 1 [-] |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminio | 9 - 11 % Show Material materials with Aluminio of 9 - 11 % | ||
Cobre | Balance | ||
Hierro | 2 - 4 % Show Material materials with Hierro of 2 - 4 % | ||
Manganeso | 1.5 % Show Material materials with Manganeso of 1.5 % | max. | |
Níquel | 4 - 5.5 % Show Material materials with Níquel of 4 - 5.5 % | ||
Silicona | 0.25 % Show Material materials with Silicona of 0.25 % |
Technological properties
Property | ||
---|---|---|
Application areas | Offshore & marine: Marine fasteners, hardware and fittings;Aerospace: Landing gear components, thrust washers, gears, control bushes, faucet balls, springs and worm wheels;Other: Non-sparking safety tooling, valve stems and seats, wear plates, welding clamps, valve spindles and components, fasteners and bearing bushes | |
Corrosion properties | High resistance to corrosion and erosion | |
General machinability | Good machinability | |
Hot forming | Easily hot worked |