General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 7.8 g/cm³ Show Material materials with Densidad of 7.8 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Charpy impact energy, V-notch | 23.0 °C | 33 J Show Material materials with Charpy impact energy, V-notch of 33 J |
Elongación | 23.0 °C | 9 - 20 % Show Material materials with Elongación of 9 - 20 % |
Límite elástico Rp 0,2 | 23.0 °C | 220 - 310 MPa Show Material materials with Límite elástico Rp 0,2 of 220 - 310 MPa |
Resistencia a la tracción | 23.0 °C | 515 - 620 MPa Show Material materials with Resistencia a la tracción of 515 - 620 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 1.8E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.8E-5 1/K | for 0-300°C |
Conductividad térmica | 23.0 °C | 45 W/(m·K) Show Material materials with Conductividad térmica of 45 W/(m·K) | |
Temperatura de fusión | 980 - 1010 °C Show Material materials with Temperatura de fusión of 980 - 1010 °C |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 23.0 °C | 4.06E+6 - 5.22E+6 S/m Show Material materials with Conductividad eléctrica of 4.06E+6 - 5.22E+6 S/m |
Specific Electrical conductivity | 7 - 8 % IACS Show Material materials with Specific Electrical conductivity of 7 - 8 % IACS |
Magnético
Property | Temperature | Value |
---|---|---|
Permeabilidad magnética relativa | 23.0 °C | 1 [-] Show Material materials with Permeabilidad magnética relativa of 1 [-] |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminio | 6 - 6.4 % Show Material materials with Aluminio of 6 - 6.4 % | ||
Cobre | Balance | ||
Hierro | 0.5 - 0.7 % Show Material materials with Hierro of 0.5 - 0.7 % | ||
Manganeso | 0.5 % Show Material materials with Manganeso of 0.5 % | max. | |
Silicona | 2 - 2.4 % Show Material materials with Silicona of 2 - 2.4 % |
Technological properties
Property | ||
---|---|---|
Application areas | Offshore & marine: High strength and non-magnetic fasteners and components;Other: Fasteners, safety tooling, valve components, non-magnetic parts, marine hardware, gears, bearings and bushes and instrumentation components | |
Corrosion properties | Excellent corrosion resistance | |
General machinability | Good machinability |