Matmatch uses cookies and similar technologies to improve your experience and measure your interactions with our website. We also use them to provide you more relevant information and improve our platform and search tools. If that’s okay, click “Accept all.” To change your preferences, click “Open cookie settings.” You will find more information about cookies on our privacy policy page.
Open cookie settings
Materiales
Categories
No estás conectado
Categories
Encontrar proveedores de metales
List Your Company
Case Studies
Tools
Sobre nosotros
BS C106 / Cu-DHP Phosphorous Deoxidised Copper
2.0090 (SF-Cu/Cu-DHP) is a grade of copper from which oxygen is removed by the controlled addition of phosphorous during the melting cycle. It is the material normally used for the manufacture of copper tubes as it can be readily welded and brazed. C106 has deep drawing characteristics superior even to those of tough pitch (C101) copper. It shows the following features and properties:
Los datos sobre este material han sido proporcionados por Matmatch.
All categories
Suppliers with similar grades
Seguridad medioambiental
Tratamiento de residuos
Sistemas mecánicos
Elementos de sujeción
Fasteners General
Sistemas de fluido
Almacenamiento de fluidos
Fluid Storage General
Tanques y contenedores
Tuberías
Energía
Mecheros y calderas
Calderas e intercambiadores de calor
Heat Exchangers In Energy
Industria química
Equipamiento para la industria química
Intercambiadores de calor
Marítimo
Estructuras navales y construcción de barcos
Sistemas de sujeción para la navegación
Producción de industria química
Industria minera
Equipos de minería
Tunnelling & Tubing
Construcción
Elementos de construcción
Tejados
Building Structures
Masonry
Instalaciones en edificios
Sistemas de calefacción central
Sistemas de ventilación y aire acondicionado
Gas Supply
Fontanería
Water Heating
Architectural Models
Bienes de consumo
Aplicaciones decorativas
Properties of Copper
List your company on Matmatch now and reach engineers around the world looking for such materials.
Request more informationChemical properties
Property | Value | Comment |
---|---|---|
Cobre | 99.85 % Show Material materials with Cobre of 99.85 % | min. |
Technological properties
Property | ||
---|---|---|
Application areas | Chemical processing: Heat exchanger plant, calorifiers, chemical plant, storage tanks, refrigeration plant, chemical pipework, water and gas installations and tubing, soil and waste disposal;Other: Roofing sheet, architectural and decorative metalwork, air conditioning equipment and pipework, central heating systems, marine and general engineering fasteners and masonry fixings | |
Corrosion properties | Good corrosion resistance |
MATMATCH
We connect engineers, product designers and procurement teams with the best materials and suppliers for their job.
EMPRESA
CONTÁCTANOS
Siebenbürger Str. 23, 86983 Lechbruck am See, Germany
© 2024 Plansee Composite Materials GmbH, All rights reserved.