Aplicaciones térmicas
Property | Value |
---|---|
Temperatura máx. de funcionamiento | 300 °C Show Material materials with Temperatura máx. de funcionamiento of 300 °C |
Chemical properties
Property | Value |
---|---|
Arsénico | 0.3 - 0.5 % Show Material materials with Arsénico of 0.3 - 0.5 % |
Cobre | Balance |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Hierro | 0.03 % Show Material materials with Hierro of 0.03 % |
Technological properties
Property | ||
---|---|---|
Application areas | Rail: Steam locomotive staybolts, rivets and boiler plates;Chemical processing: Chemical plant and equipment for relatively non-corrosive liquids and gases at moderately elevated temperatures | |
Corrosion properties | Good corrosion resistance |