General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 8.95 g/cm³ Show Material materials with Densidad of 8.95 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 23.0 °C | 80 - 120 [-] Show Material materials with Dureza Brinell of 80 - 120 [-] |
Elongación | 23.0 °C | 27 - 30 % Show Material materials with Elongación of 27 - 30 % |
Límite elástico Rp 0,2 | 23.0 °C | 125 MPa Show Material materials with Límite elástico Rp 0,2 of 125 MPa |
Módulo de cizallamiento | 23.0 °C | 56 GPa Show Material materials with Módulo de cizallamiento of 56 GPa |
Módulo elástico | 23.0 °C | 152 GPa Show Material materials with Módulo elástico of 152 GPa |
Resistencia a la tracción | 23.0 °C | 310 - 330 MPa Show Material materials with Resistencia a la tracción of 310 - 330 MPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Calor específico | 23.0 °C | 377 J/(kg·K) Show Material materials with Calor específico of 377 J/(kg·K) |
Coeficiente de dilatación térmica | 23.0 °C | 1.6E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.6E-5 1/K |
Conductividad térmica | 23.0 °C | 29 W/(m·K) Show Material materials with Conductividad térmica of 29 W/(m·K) |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 23.0 °C | 2.90E+6 S/m Show Material materials with Conductividad eléctrica of 2.90E+6 S/m |
Resistividad eléctrica | 23.0 °C | 3.4E-7 Ω·m Show Material materials with Resistividad eléctrica of 3.4E-7 Ω·m |
Specific Electrical conductivity | 5 % IACS Show Material materials with Specific Electrical conductivity of 5 % IACS |
Chemical properties
Technological properties
Property | ||
---|---|---|
Application areas | Offshore & marine: Salt water flanges, salt water piping and pipe fittings, valve bodies, sea water intakes, pipe fittings, water boxes, propeller sleeves, pump bodies and parts;Chemical processing: Heat exchanger and cooling plant, evaporator tubes, distiller tubes, refrigerator and condenser components;Other: Welding backing rings, flexible metal hose, weld wire and boiler parts | |
Cold Forming | Good cold formability | |
Corrosion properties | Excellent corrosion and pitting resistance in marine environments | |
General machinability | Easily machined, Machinability rating: 20 | |
Hot forming | Good hot formability with hot working temperature between 925-1025°C. |