General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 8.5 g/cm³ Show Material materials with Densidad of 8.5 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 23.0 °C | 229 - 240 [-] Show Material materials with Dureza Brinell of 229 - 240 [-] |
Elongación | 23.0 °C | 12 % Show Material materials with Elongación of 12 % |
Límite elástico Rp 0,2 | 23.0 °C | 555 - 630 MPa Show Material materials with Límite elástico Rp 0,2 of 555 - 630 MPa |
Módulo elástico | 23.0 °C | 141 GPa Show Material materials with Módulo elástico of 141 GPa |
Resistencia a la tracción | 23.0 °C | 770 - 850 MPa Show Material materials with Resistencia a la tracción of 770 - 850 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 1.64E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.64E-5 1/K | for 0-400°C |
Conductividad térmica | 23.0 °C | 44 - 46 W/(m·K) Show Material materials with Conductividad térmica of 44 - 46 W/(m·K) | |
Temperatura de fusión | 1080 - 1100 °C Show Material materials with Temperatura de fusión of 1080 - 1100 °C |
Eléctrico
Property | Temperature | Value |
---|---|---|
Resistividad eléctrica | 23.0 °C | 1.7E-7 Ω·m Show Material materials with Resistividad eléctrica of 1.7E-7 Ω·m |
Magnético
Property | Temperature | Value | Comment |
---|---|---|---|
Permeabilidad magnética relativa | 23.0 °C | 1 [-] Show Material materials with Permeabilidad magnética relativa of 1 [-] | max. |
Chemical properties
Technological properties
Property | ||
---|---|---|
Application areas | Offshore & marine: Marine shafts and bearing bushes, offshore bolting, valve and pump trim;Aerospace: Aircraft landing gear bushes, actuating sleeves, steering gear, bearing bushes, non-magnetic bolts and control surface components;Automotive: High performance engine shafts, gears, pinions, bearing bushes, locking nuts, mechanical and electromechanical components, thrust washers and hydraulic equipment;Chemical processing: Pump and valve spindles and other trim, flanges, pipe fittings, clamps and plant components | |
Corrosion properties | Excellent corrosion resistance | |
General machinability | Good machinability |