2.0857 (CuNi3Si) ultimate super strength copper nickel silicon alloy, specially developed to provide a unique blend of mechnical and physical properties for high performance engineering. It has similar characteristics to Colsibro®, although Trojan is produced with increased levels of nickel and silicon in order to further increase the mechanical strength. It shows the following features and properties:


  • Ultra-high strength
  • High electrical and thermal conductivity
  • Excellent wear and galling resistance
  • Extremely low magnetic permeability
  • Excellent general corrosion resistance
  • Outstanding bearing properties
  • Spark resistance
  • Good machinability and dimensional stability
  • Outstanding low temperature mechanical properties
  • Related Standards

    Equivalent Materials

    Los datos sobre este material han sido proporcionados por Matmatch.

    A menos que se indique lo contrario, todas las medidas corresponden a condiciones de temperatura ambiente. A menos que se indique lo contrario, se utilizan las unidades del SI.
    Las normas armonizadas son similares a uno o varios estándares del proveedor. Es posible que algunas normas armonizadas se ajusten al estándar original, mientras que otras pueden quedar fuera de su alcance.

    Ashby charts

    Propiedades

    General

    PropertyTemperatureValue

    Densidad

    23.0 °C

    8.8 g/cm³

    Show Material materials with Densidad of 8.8 g/cm³

    Mecánica

    PropertyTemperatureValue

    Dureza Brinell

    23.0 °C

    190 - 200 [-]

    Show Material materials with Dureza Brinell of 190 - 200 [-]

    Elongación

    23.0 °C

    10 %

    Show Material materials with Elongación of 10 %

    Límite elástico Rp 0,2

    23.0 °C

    570 - 750 MPa

    Show Material materials with Límite elástico Rp 0,2 of 570 - 750 MPa

    Resistencia a la tracción

    23.0 °C

    690 - 800 MPa

    Show Material materials with Resistencia a la tracción of 690 - 800 MPa

    Aplicaciones térmicas

    PropertyTemperatureValueComment

    Coeficiente de dilatación térmica

    23.0 °C

    1.6E-5 1/K

    Show Material materials with Coeficiente de dilatación térmica of 1.6E-5 1/K

    for 0-400°C

    Conductividad térmica

    23.0 °C

    159 W/(m·K)

    Show Material materials with Conductividad térmica of 159 W/(m·K)

    Temperatura de fusión

    1060 - 1085 °C

    Show Material materials with Temperatura de fusión of 1060 - 1085 °C

    Eléctrico

    PropertyTemperatureValue

    Conductividad eléctrica

    23.0 °C

    1.74E+7 S/m

    Show Material materials with Conductividad eléctrica of 1.74E+7 S/m

    Specific Electrical conductivity

    30 % IACS

    Show Material materials with Specific Electrical conductivity of 30 % IACS

    Magnético

    PropertyTemperatureValue

    Permeabilidad magnética relativa

    23.0 °C

    1 [-]

    Show Material materials with Permeabilidad magnética relativa of 1 [-]

    Chemical properties

    PropertyValue

    Cobre

    Balance

    Níquel

    2.6 - 4.5 %

    Show Material materials with Níquel of 2.6 - 4.5 %

    Silicona

    0.8 - 1.3 %

    Show Material materials with Silicona of 0.8 - 1.3 %

    Technological properties

    Property
    Application areas

    Automotive: valve guides, bushes and valve seats;Electrical: current-carrying electrical components such as slip rings, squirrel cages, springs, rotary switch contacts, contact blades, short-circuit rings and heavy duty switchgear;Offshore & marine: Downhole tools, shear pins, hydraulic valve bodies, pump components and ball valves and mechanical seals;Other: Non-magnetic tooling, plastic mould tooling, friction pads and fibre optic connectors

    Corrosion properties

    Excellent corrosion resistance

    General machinability

    Good machinability