General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 8.26 g/cm³ Show Material materials with Densidad of 8.26 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Rockwell C | 23.0 °C | 36 - 42 [-] Show Material materials with Dureza Rockwell C of 36 - 42 [-] |
Elongación | 23.0 °C | 3 % Show Material materials with Elongación of 3 % |
Límite elástico Rp 0,2 | 23.0 °C | 900 MPa Show Material materials with Límite elástico Rp 0,2 of 900 MPa |
Módulo de cizallamiento | 23.0 °C | 50 GPa Show Material materials with Módulo de cizallamiento of 50 GPa |
Módulo elástico | 23.0 °C | 130 GPa Show Material materials with Módulo elástico of 130 GPa |
Resistencia a la tracción | 23.0 °C | 1140 - 1380 MPa Show Material materials with Resistencia a la tracción of 1140 - 1380 MPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Conductividad térmica | 23.0 °C | 84 - 130 W/(m·K) Show Material materials with Conductividad térmica of 84 - 130 W/(m·K) |
Eléctrico
Property | Temperature | Value |
---|---|---|
Resistividad eléctrica | 23.0 °C | 7.9E-8 Ω·m Show Material materials with Resistividad eléctrica of 7.9E-8 Ω·m |
Specific Electrical conductivity | 25 % IACS Show Material materials with Specific Electrical conductivity of 25 % IACS |
Chemical properties
Technological properties
Property | ||
---|---|---|
Application areas | Aerospace: Landing gear, bearing bushes and high performance fasteners;Automotive: Valve guides, bushes and valve seats;Offshore & marine: Offshore drilling and instrumentation equipment, downhole tooling, valve, pump and shaft components;Other: Deep drawing tooling, plastic moulding dies, tools and plungers, die-casting plunger tips, non-magnetic and non sparking tools, electrical and electronic connectors, springs, fasteners, switchgear, resistance welding electrodes and equipment, flash butt welding dies and inserts, seam welding electrode shafts | |
Corrosion properties | High corrosion resistance | |
General machinability | Very good machinability |