Mecánica
Chemical properties
Technological properties
Property | ||
---|---|---|
Application areas | Chemical processing: Phosphoric acid evaporators, pickling-tank heaters, pickling hooks and equipment, and chemical process equipment;Power generation: Components for spent nuclear fuel element recovery;Other: Tank trucks and propeller shafts | |
Corrosion properties | Excellent corrosion resistance | |
General machinability | It is readily machinable |