General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 8.47 g/cm³ Show Material materials with Densidad of 8.47 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Vickers | 23.0 °C | 130 [-] Show Material materials with Dureza Vickers of 130 [-] |
Elongación | 23.0 °C | 20 % Show Material materials with Elongación of 20 % |
Límite elástico Rp 0,2 | 23.0 °C | 230 MPa Show Material materials with Límite elástico Rp 0,2 of 230 MPa |
Módulo elástico | 23.0 °C | 100 GPa Show Material materials with Módulo elástico of 100 GPa |
Resistencia a la tracción | 23.0 °C | 520 MPa Show Material materials with Resistencia a la tracción of 520 MPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Conductividad térmica | 23.0 °C | 46 W/(m·K) Show Material materials with Conductividad térmica of 46 W/(m·K) |
Temperatura de fusión | 940 - 980 °C Show Material materials with Temperatura de fusión of 940 - 980 °C |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 23.0 °C | 5.22E+6 S/m Show Material materials with Conductividad eléctrica of 5.22E+6 S/m |
Resistividad eléctrica | 23.0 °C | 1.8E-7 Ω·m Show Material materials with Resistividad eléctrica of 1.8E-7 Ω·m |
Specific Electrical conductivity | 9 % IACS Show Material materials with Specific Electrical conductivity of 9 % IACS |
Magnético
Property | Temperature | Value | Comment |
---|---|---|---|
Permeabilidad magnética relativa | 23.0 °C | 1.05 [-] Show Material materials with Permeabilidad magnética relativa of 1.05 [-] | max. |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Cobre | 44 - 47 % Show Material materials with Cobre of 44 - 47 % | ||
Hierro | 0.4 % Show Material materials with Hierro of 0.4 % | max. | |
Manganeso | 0.2 - 0.5 % Show Material materials with Manganeso of 0.2 - 0.5 % | ||
Níquel | 9 - 11 % Show Material materials with Níquel of 9 - 11 % | ||
Plomo | 1 - 2.5 % Show Material materials with Plomo of 1 - 2.5 % | ||
Zinc | Balance |
Technological properties
Property | ||
---|---|---|
Application areas | Frequently used applications of NS101 include gears, pinions, clock and watch parts, screws and other types of fasteners, hot stampings and forgings, keys, lock parts, door furniture, grills, decorative and architectural metalwork, darts, fishing tackle, camera, binocular and microscope parts, musical instrument valves and fittings, electrical and electronic pins and connectors and switchgear components. | |
Corrosion properties | Good corrosion resistance | |
General machinability | Very good machining and hot stamping characteristics |