General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 8.44 g/cm³ Show Material materials with Densidad of 8.44 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Vickers | 23.0 °C | 185 [-] Show Material materials with Dureza Vickers of 185 [-] |
Elongación | 23.0 °C | 20 % Show Material materials with Elongación of 20 % |
Límite elástico Rp 0,2 | 23.0 °C | 450 MPa Show Material materials with Límite elástico Rp 0,2 of 450 MPa |
Módulo elástico | 23.0 °C | 120 GPa Show Material materials with Módulo elástico of 120 GPa |
Resistencia a la tracción | 23.0 °C | 560 MPa Show Material materials with Resistencia a la tracción of 560 MPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Conductividad térmica | 23.0 °C | 30 W/(m·K) Show Material materials with Conductividad térmica of 30 W/(m·K) |
Temperatura de fusión | 850 - 870 °C Show Material materials with Temperatura de fusión of 850 - 870 °C |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 23.0 °C | 2.90E+6 S/m Show Material materials with Conductividad eléctrica of 2.90E+6 S/m |
Resistividad eléctrica | 23.0 °C | 3.4E-7 Ω·m Show Material materials with Resistividad eléctrica of 3.4E-7 Ω·m |
Specific Electrical conductivity | 5 % IACS Show Material materials with Specific Electrical conductivity of 5 % IACS |
Magnético
Property | Temperature | Value | Comment |
---|---|---|---|
Permeabilidad magnética relativa | 23.0 °C | 1.05 [-] Show Material materials with Permeabilidad magnética relativa of 1.05 [-] | max. |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Cobre | 47 - 50 % Show Material materials with Cobre of 47 - 50 % | ||
Hierro | 0.3 % Show Material materials with Hierro of 0.3 % | max. | |
Manganeso | 1.5 - 3 % Show Material materials with Manganeso of 1.5 - 3 % | ||
Níquel | 6 - 8 % Show Material materials with Níquel of 6 - 8 % | ||
Plomo | 2.3 - 3.3 % Show Material materials with Plomo of 2.3 - 3.3 % | ||
Zinc | Balance |
Technological properties
Property | ||
---|---|---|
Application areas | General: Gears, pinions, clock and watch parts, screws and fasteners, keys, lock parts, decorative and architectural metalwork, camera parts, electrical and electronic pins and connectors, medical, industrial and scientific instrument components | |
Corrosion properties | Very high corrosion resistance | |
General machinability | Excellent machinability |