General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 7.8 g/cm³ Show Material materials with Densidad of 7.8 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.32 [-] Show Material materials with Coeficiente de Poisson of 0.32 [-] | |
Dureza Brinell | 23.0 °C | 270 [-] Show Material materials with Dureza Brinell of 270 [-] | max. |
Elongación | 23.0 °C | 25 % Show Material materials with Elongación of 25 % | |
Límite elástico Rp 0,2 | 23.0 °C | 550 MPa Show Material materials with Límite elástico Rp 0,2 of 550 MPa | |
Módulo de cizallamiento | 23.0 °C | 75 GPa Show Material materials with Módulo de cizallamiento of 75 GPa | |
Módulo elástico | 23.0 °C | 199 GPa Show Material materials with Módulo elástico of 199 GPa | |
Resistencia a la tracción | 23.0 °C | 750 MPa Show Material materials with Resistencia a la tracción of 750 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 425 J/(kg·K) Show Material materials with Calor específico of 425 J/(kg·K) | |
Coeficiente de dilatación térmica | 23.0 °C | 1.11E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.11E-5 1/K | for 20-100°C |
Conductividad térmica | 23.0 °C | 14 W/(m·K) Show Material materials with Conductividad térmica of 14 W/(m·K) | for 20-300°C |
Eléctrico
Property | Temperature | Value |
---|---|---|
Resistividad eléctrica | 23.0 °C | 8E-7 Ω·m Show Material materials with Resistividad eléctrica of 8E-7 Ω·m |
Magnético
Property | Temperature | Value |
---|---|---|
Permeabilidad magnética relativa | 23.0 °C | 33 [-] Show Material materials with Permeabilidad magnética relativa of 33 [-] |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Azufre | 0.01 % Show Material materials with Azufre of 0.01 % | max. | |
Carbono | 0.03 % Show Material materials with Carbono of 0.03 % | max. | |
Cobre | 0.5 - 1 % Show Material materials with Cobre of 0.5 - 1 % | ||
Cromo | 24 - 26 % Show Material materials with Cromo of 24 - 26 % | ||
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % | max. | |
Hierro | Balance | ||
Manganeso | 1 % Show Material materials with Manganeso of 1 % | max. | |
Molibdeno | 3 - 4 % Show Material materials with Molibdeno of 3 - 4 % | ||
Nitrógeno | 0.2 - 0.3 % Show Material materials with Nitrógeno of 0.2 - 0.3 % | ||
Níquel | 6 - 8 % Show Material materials with Níquel of 6 - 8 % | ||
Silicona | 1 % Show Material materials with Silicona of 1 % | max. | |
Wolframio | 0.5 - 1 % Show Material materials with Wolframio of 0.5 - 1 % |
Technological properties
Property | ||
---|---|---|
Application areas | Offshore & marine: Offshore platforms, components for gas, oil and process cooling plants, instrumentation, wellhead and subsea wellhead fittings, desalination plants, seawater cooled heat exchangers, cargo heating systems, marine shafts (for boats etc) and high strength fasteners;Chemical processing: Equipment handling organic or dilute sulphuric acid, process solutions contaminated with chlorides, refinery equipment, desulphurising and distillation units, sewage plant components, fire extinguishing systems, general processing and mixing plant | |
Corrosion properties | Very good corrosion resistance |