Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 23.0 °C | 255 - 321 [-] Show Material materials with Dureza Brinell of 255 - 321 [-] |
Elongación | 23.0 °C | 12 % Show Material materials with Elongación of 12 % |
Límite elástico | 23.0 °C | 690 MPa Show Material materials with Límite elástico of 690 MPa |
Resistencia a la tracción | 23.0 °C | 880 - 1080 MPa Show Material materials with Resistencia a la tracción of 880 - 1080 MPa |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Carbono | 0.16 % Show Material materials with Carbono of 0.16 % | max. | |
Cromo | 16.5 % Show Material materials with Cromo of 16.5 % | ||
Hierro | Balance | ||
Manganeso | 0.3 % Show Material materials with Manganeso of 0.3 % | ||
Níquel | 2.5 % Show Material materials with Níquel of 2.5 % | ||
Silicona | 0.25 % Show Material materials with Silicona of 0.25 % |
Technological properties
Property | ||
---|---|---|
Application areas | Offshore & marine: High strength fasteners, bolts and shafts;Aerospace: Various aerospace components including high strength fasteners;Other: Compressor forms, dairies, machine tool industry, marine engineering, paper mills, plant engineering, starch mills and yeast factories | |
Corrosion properties | Excellent corrosion resistance |