Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 23.0 °C | 140 - 220 [-] Show Material materials with Dureza Brinell of 140 - 220 [-] |
Elongación | 23.0 °C | 35 % Show Material materials with Elongación of 35 % |
Límite elástico | 23.0 °C | 210 MPa Show Material materials with Límite elástico of 210 MPa |
Resistencia a la tracción | 23.0 °C | 540 MPa Show Material materials with Resistencia a la tracción of 540 MPa |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Carbono | 0.08 % Show Material materials with Carbono of 0.08 % | max. | |
Cromo | 18 % Show Material materials with Cromo of 18 % | ||
Hierro | Balance | ||
Manganeso | 1 % Show Material materials with Manganeso of 1 % | ||
Molibdeno | 1 % Show Material materials with Molibdeno of 1 % | max. | |
Niobio | 1.1 % Show Material materials with Niobio of 1.1 % | max. | |
Níquel | 9 % Show Material materials with Níquel of 9 % |
Technological properties
Property | ||
---|---|---|
Application areas | Aerospace: Aerospace components and fasteners;Other: Breweries, cellulose, industry, dairies, fermentation industry, food processing, leather industry, machine tool industries, nitric acid plants, nuclear engineering, paper mills and production of explosives | |
Cold Forming | Good cold working characteristics | |
Corrosion properties | High corrosion resistance |