Chemical properties
Property | Value | Comment | |
---|---|---|---|
Carbono | 0.07 % Show Material materials with Carbono of 0.07 % | max. | |
Cobre | 1.6 % Show Material materials with Cobre of 1.6 % | ||
Cromo | 14 % Show Material materials with Cromo of 14 % | ||
Hierro | Balance | ||
Manganeso | 1 % Show Material materials with Manganeso of 1 % | max. | |
Molibdeno | 1.6 % Show Material materials with Molibdeno of 1.6 % | max. | |
Níquel | 5.4 % Show Material materials with Níquel of 5.4 % | ||
Silicona | 0.6 % Show Material materials with Silicona of 0.6 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Aerospace: Gas turbine blades, undercarriage components and fasteners | |
Corrosion properties | Good general corrosion resistance |