General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 8.74 g/cm³ Show Material materials with Densidad of 8.74 g/cm³ |
Medidas
Property | Value | Comment | |
---|---|---|---|
Ancho | 3.2 - 31.8 mm Show Material materials with Ancho of 3.2 - 31.8 mm | ||
Longitud | 3050 - 3660 mm Show Material materials with Longitud of 3050 - 3660 mm | Mill random length | |
Dimensions | Available widths: 3.2mm, 3.6mm, 6.4mm, 12.7mm, 15.9mm, 19.1mm, 25.4mm, 31.8mm |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Rockwell B | 23.0 °C | 85 [-] Show Material materials with Dureza Rockwell B of 85 [-] | |
Elongación | 23.0 °C | 40 % Show Material materials with Elongación of 40 % | in 2 in. |
Límite elástico | 23.0 °C | 262 MPa Show Material materials with Límite elástico of 262 MPa | |
Módulo elástico | 23.0 °C | 217 GPa Show Material materials with Módulo elástico of 217 GPa | |
Resistencia a la tracción | 23.0 °C | 676 MPa Show Material materials with Resistencia a la tracción of 676 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 460 J/(kg·K) Show Material materials with Calor específico of 460 J/(kg·K) | |
Coeficiente de dilatación térmica | 450.0 °C | 1.36E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.36E-5 1/K | from 20°C to the mentioned temperature |
Conductividad térmica | 23.0 °C | 35 W/(m·K) Show Material materials with Conductividad térmica of 35 W/(m·K) | |
Temperatura de fusión | 1454 °C Show Material materials with Temperatura de fusión of 1454 °C |
Eléctrico
Property | Temperature | Value |
---|---|---|
Resistividad eléctrica | 23.0 °C | 5.9E-7 Ω·m Show Material materials with Resistividad eléctrica of 5.9E-7 Ω·m |
Magnético
Property | Temperature | Value |
---|---|---|
Fuerza coercitiva | 23.0 °C | 1.19 A/m Show Material materials with Fuerza coercitiva of 1.19 A/m |
Inducción de saturación | 23.0 °C | 0.8 T Show Material materials with Inducción de saturación of 0.8 T |
Permeabilidad magnética relativa | 23.0 °C | 230000 [-] Show Material materials with Permeabilidad magnética relativa of 230000 [-] |
Temperatura de Curie | 460 °C Show Material materials with Temperatura de Curie of 460 °C |
Chemical properties
Property | Value |
---|---|
Azufre | 8E-3 % Show Material materials with Azufre of 8E-3 % |
Carbono | 0.03 % Show Material materials with Carbono of 0.03 % |
Fósforo | 0.02 % Show Material materials with Fósforo of 0.02 % |
Hierro | Balance |
Manganeso | 0.95 % Show Material materials with Manganeso of 0.95 % |
Molibdeno | 5 % Show Material materials with Molibdeno of 5 % |
Níquel | 80 % Show Material materials with Níquel of 80 % |
Silicona | 0.42 % Show Material materials with Silicona of 0.42 % |
Technological properties
Property | ||
---|---|---|
Application areas | Common applications of EFI ALLOY 79 are: Toroidal tape-wound cores - instrument transformers, inductive components, earth-leakage circuit breakers; Magnetic shielding - shielding cans, shielding films, spatial shielding arrangements; Ground fault circuit interrupters; Electromagnetic relay parts; Laminations - transformer laminations, transformer cores for modems, stampled rings for electronic earth-leakage breakers, operating at a low magnetic field strengths |