General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 8.17 g/cm³ Show Material materials with Densidad of 8.17 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Rockwell B | 23.0 °C | 80 [-] Show Material materials with Dureza Rockwell B of 80 [-] | |
Elongación | 23.0 °C | 30 % Show Material materials with Elongación of 30 % | in 2 in. |
Límite elástico | 23.0 °C | 242 MPa Show Material materials with Límite elástico of 242 MPa | |
Módulo elástico | 23.0 °C | 159 GPa Show Material materials with Módulo elástico of 159 GPa | |
Resistencia a la tracción | 23.0 °C | 552 MPa Show Material materials with Resistencia a la tracción of 552 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 502 J/(kg·K) Show Material materials with Calor específico of 502 J/(kg·K) | |
Coeficiente de dilatación térmica | 100.0 °C | 8.2E-6 1/K Show Material materials with Coeficiente de dilatación térmica of 8.2E-6 1/K | from 30°C to the mentioned temperature |
150.0 °C | 8.1E-6 1/K Show Material materials with Coeficiente de dilatación térmica of 8.1E-6 1/K | from 30°C to the mentioned temperature | |
200.0 °C | 7.9E-6 1/K Show Material materials with Coeficiente de dilatación térmica of 7.9E-6 1/K | from 30°C to the mentioned temperature | |
250.0 °C | 7.8E-6 1/K Show Material materials with Coeficiente de dilatación térmica of 7.8E-6 1/K | from 30°C to the mentioned temperature | |
300.0 °C | 7.5E-6 1/K Show Material materials with Coeficiente de dilatación térmica of 7.5E-6 1/K | from 30°C to the mentioned temperature | |
350.0 °C | 7.1E-6 - 7.8E-6 1/K Show Material materials with Coeficiente de dilatación térmica of 7.1E-6 - 7.8E-6 1/K | from 30°C to the mentioned temperature | |
375.0 °C | 7.5E-6 1/K Show Material materials with Coeficiente de dilatación térmica of 7.5E-6 1/K | from 30°C to the mentioned temperature | |
400.0 °C | 7.5E-6 1/K Show Material materials with Coeficiente de dilatación térmica of 7.5E-6 1/K | from 30°C to the mentioned temperature | |
425.0 °C | 7.6E-6 1/K Show Material materials with Coeficiente de dilatación térmica of 7.6E-6 1/K | from 30°C to the mentioned temperature | |
450.0 °C | 7.9E-6 1/K Show Material materials with Coeficiente de dilatación térmica of 7.9E-6 1/K | from 30°C to the mentioned temperature | |
500.0 °C | 8.2E-6 - 8.9E-6 1/K Show Material materials with Coeficiente de dilatación térmica of 8.2E-6 - 8.9E-6 1/K | from 30°C to the mentioned temperature | |
550.0 °C | 9.3E-6 1/K Show Material materials with Coeficiente de dilatación térmica of 9.3E-6 1/K | from 30°C to the mentioned temperature | |
600.0 °C | 9.8E-6 1/K Show Material materials with Coeficiente de dilatación térmica of 9.8E-6 1/K | from 30°C to the mentioned temperature | |
700.0 °C | 1.07E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.07E-5 1/K | from 30°C to the mentioned temperature | |
800.0 °C | 1.16E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.16E-5 1/K | from 30°C to the mentioned temperature | |
900.0 °C | 1.25E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.25E-5 1/K | from 30°C to the mentioned temperature | |
1000.0 °C | 1.34E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.34E-5 1/K | from 30°C to the mentioned temperature | |
Conductividad térmica | 23.0 °C | 11 W/(m·K) Show Material materials with Conductividad térmica of 11 W/(m·K) | |
Temperatura de fusión | 1427 °C Show Material materials with Temperatura de fusión of 1427 °C |
Eléctrico
Property | Temperature | Value |
---|---|---|
Resistividad eléctrica | 23.0 °C | 4.7E-7 Ω·m Show Material materials with Resistividad eléctrica of 4.7E-7 Ω·m |
Magnético
Property | Value |
---|---|
Temperatura de Curie | 460 °C Show Material materials with Temperatura de Curie of 460 °C |
Chemical properties
Property | Value |
---|---|
Azufre | 0.025 % Show Material materials with Azufre of 0.025 % |
Carbono | 0.05 % Show Material materials with Carbono of 0.05 % |
Cromo | 0.03 % Show Material materials with Cromo of 0.03 % |
Hierro | Balance |
Manganeso | 0.5 % Show Material materials with Manganeso of 0.5 % |
Níquel | 46 % Show Material materials with Níquel of 46 % |
Silicona | 0.3 % Show Material materials with Silicona of 0.3 % |
Technological properties
Property | ||
---|---|---|
Application areas | Common applications of Alloy 42: Thermostats, thermoswitches, integrated circuit lead frames, select glass-to-metal sealing applications, high temperature curing of aircraft thermoset composites |