General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 8.89 g/cm³ Show Material materials with Densidad of 8.89 g/cm³ |
Medidas
Property | Value |
---|---|
Ancho | 3.18 - 57.2 mm Show Material materials with Ancho of 3.18 - 57.2 mm |
Dimensions | Available widths: 3.2mm, 4.8mm, 6.4mm, 7.9mm, 9.5mm, 12.7mm, 15.9mm, 19.1mm, 22.2mm, 28.6mm, 31.8mm, 44.5mm, 50.8mm, 57.2mm |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Rockwell B | 23.0 °C | 80 [-] Show Material materials with Dureza Rockwell B of 80 [-] | |
Elongación | 23.0 °C | 40 % Show Material materials with Elongación of 40 % | in 2 in. |
Límite elástico | 23.0 °C | 138 MPa Show Material materials with Límite elástico of 138 MPa | |
Módulo elástico | 23.0 °C | 207 GPa Show Material materials with Módulo elástico of 207 GPa | |
Resistencia a la tracción | 23.0 °C | 449 MPa Show Material materials with Resistencia a la tracción of 449 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 452 J/(kg·K) Show Material materials with Calor específico of 452 J/(kg·K) | |
Coeficiente de dilatación térmica | 100.0 °C | 1.3E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.3E-5 1/K | from 30°C to the mentioned temperature |
Conductividad térmica | 23.0 °C | 79 W/(m·K) Show Material materials with Conductividad térmica of 79 W/(m·K) | |
Temperatura de fusión | 1440 °C Show Material materials with Temperatura de fusión of 1440 °C |
Eléctrico
Property | Temperature | Value |
---|---|---|
Resistividad eléctrica | 23.0 °C | 8.5E-8 Ω·m Show Material materials with Resistividad eléctrica of 8.5E-8 Ω·m |
Magnético
Property | Value |
---|---|
Temperatura de Curie | 360 °C Show Material materials with Temperatura de Curie of 360 °C |
Chemical properties
Property | Value |
---|---|
Azufre | 0.01 % Show Material materials with Azufre of 0.01 % |
Carbono | 0.02 % Show Material materials with Carbono of 0.02 % |
Hierro | 0.25 % Show Material materials with Hierro of 0.25 % |
Níquel | 99.5 % Show Material materials with Níquel of 99.5 % |
Silicona | 0.25 % Show Material materials with Silicona of 0.25 % |
Technological properties
Property | ||
---|---|---|
Application areas | Common applications of Nickel 201: Getter tabs, heating element sheathing, anodes, fuel cells, special purpose electron tubes, transistor enclosures, cathode shields, spark gaps |