General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 17.5 g/cm³ Show Material materials with Densidad of 17.5 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Rockwell C | 23.0 °C | 33 [-] Show Material materials with Dureza Rockwell C of 33 [-] |
Elongación | 23.0 °C | 2 % Show Material materials with Elongación of 2 % |
Límite elástico | 23.0 °C | 517 MPa Show Material materials with Límite elástico of 517 MPa |
Módulo elástico | 23.0 °C | 331 GPa Show Material materials with Módulo elástico of 331 GPa |
Resistencia a la tracción | 23.0 °C | 648 MPa Show Material materials with Resistencia a la tracción of 648 MPa |
Chemical properties
Property | Value |
---|---|
Wolframio | 92.5 % Show Material materials with Wolframio of 92.5 % |
Technological properties
Property | ||
---|---|---|
Application areas | Common applications of Tungsten Alloys: Radiation shielding, boring bars, counterweights in aircraft and racing cars |