General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 7.4 g/cm³ Show Material materials with Densidad of 7.4 g/cm³ |
Aplicaciones térmicas
Property | Value |
---|---|
Temperatura de fusión | 232 °C Show Material materials with Temperatura de fusión of 232 °C |
Chemical properties
Property | Value |
---|---|
Cobre | 0.01 - 1 % Show Material materials with Cobre of 0.01 - 1 % |
Cromo | 2 - 6 % Show Material materials with Cromo of 2 - 6 % |
Estaño | 90 - 100 % Show Material materials with Estaño of 90 - 100 % |
Plata | 3 - 5 % Show Material materials with Plata of 3 - 5 % |
Technological properties
Property | ||
---|---|---|
Certifications | RoHS | |
Other | The key features are: Excellent flow, good wetting of surfaces to be joined, electrically and thermally conductive, aluminium to aluminium can be soldered without using flux, carbon can be soldered to metals (e.g. copper, aluminium), ceramics and glass materials, C-Solder is not affected by cleaning solvents, C-Solder does not leave residues, C-Solder is not flammable, C-Solder is flux free, C-Solder is lead free |